3D Printing Casting Photosensitive Resin (405nm UV) | WR-JC
Wax Content 30–40% | Excellent Flammability
Small Expansion | No Residue
VNICI MATERIALS
| Maximum force (KGF) | 88.6±10% |
| Tensile strength (MPA) | 20.88±10% |
| Deformation of maximum force point (MM) | 18.73±10% |
| Yield point elongation (%) | 47.34±10% |
| Elongation at break (%) | 32.96±10% |
| Maximum Flexural Strength (MPA) | 13.75±10% |
| Flexural Modulus of Elasticity (MPA) | 333.68±10% |
| Hardness (Shore D) | 58~68 |
| Impact strength, notched Izod, J/M | 117.72±10% |
| Tensile modulus (MPA) | 152.82±10% |
| Series | Ordinary Casting Resin |
| Model | WR-JC |
| Color | Green |
| Recommended Bottom Expose Time(Light Intensity 3500~4500μw/cm²) | 40~50S |
| Recommended Expose time(Light Intensity 3500~4500μw/cm²) | 8~ 12S |
| Bottom Lift Distance | 6mm |
| Lifting Distance | 6mm |
| Bottom Lift Speed | 60mm/min |
| Lift Speed | 80mm/min |
| Retract Speed | 150mm/min |
| Absorption Band | 385~410nm |