3D Printing Denture Base Photosensitive Resin (405nm UV) | WR-DB
Customizable Colors | Batch-Based Packaging
Delivery Inspection Recommended | Clear Receipt Policy
VNICI MATERIALS
| Parameter | Value |
| Maximum force (KGF) | 108.7±10% |
| Tensile strength (MPa) | 25.62±10% |
| Deformation at maximum force point (mm) | 9.99±10% |
| Yield point elongation (%) | 5.50±10% |
| Elongation at break (%) | 17.65±10% |
| Maximum bending strength (MPa) | 25.48±10% |
| Flexural modulus of elasticity (MPa) | 693.51±10% |
| Shore hardness (D) | 80-85 |
| Impact strength (j/m) | 118.46±10% |
| Tensile modulus (MPa) | 320.80+10% |
| Temperature | 23±2°C |
| Relative humidity | 50%RH±5%RH |
| Test Spline Standard | ASTM |
| Post-curing conditions | Put the test strip in water and cure the front and back sides for 1 minute under the 405 band ultraviolet light of 200 mw/cm. |
| Series | Denture Base Resin |
| Model | WR-DB |
| Color | Pink |
| Recommended Bottom Expose Time (Light Intensity 3500~4500μw/cm²) | 20~30S |
| Recommended Expose time (Light Intensity 3500~4500μw/cm²) | 3~6S |
| Bottom Lift Distance | 6mm |
| Lifting Distance | 6mm |
| Bottom Lift Speed | 60mm/min |
| Lift Speed | 80mm/min |
| Retract Speed | 150mm/min |
| Absorption Band | 385~410nm |